Show full item recordAbstract
Quality of resiperene 35 highly dependent on the quality of rubber raw materials SIR
10. One of the parameters used in determining the quality of SIR 10 quality rubber
that is the determination of moisture content is more or less content will affect quality
of the product is good resiprene viscosity and colors.
This analysis is very effective because it will give you an idea of how the product is
actually produced. From the experimental data obtained by the influence of moisture
content of raw materials for the quality of SIR 10 resiprene ie viscosities from 35 to
0.51% - 0.63%, its viscosity was increased, the viscosity decreased 0.65%, the
viscosity increased by 0.72% again, and from 0.72% - 0.97%, its viscosity falls. While
for quality color lovibond resiprene using tools to analyze the color, the color got all
nearly in the range of 11 bright brownish yellow, except at 0.54% there is obtained
between 11 and 12 rather dark brownish yellow.