    Efektivitas Defibrilasi pada Isolasi Nanoserat Selulosa Batang Eceng Gondok (Eichornia Crassipes) melalui Perlakuan Awal Ledak Uap dan Variasi Waktu Ultrasonikasi

    Effectiveness of Defibrillation on the Cellulose Nanofibers Isolation from Water Hyacinth (Eichornia Crassipes) Stem by Steam Explosion Pretreatment and Ultrasonication with Time Variation

    Thumbnail
    View/Open
    Cover (394.9Kb)
    Fulltext (6.136Mb)
    Date
    2024
    Author
    Ibadurrahman, Muhammad
    Advisor(s)
    Gea, Saharman
    Metadata
    Show full item record
    Abstract
    Water hyacinth is among the world's top 10 invasive weeds due to its adaptability and high growth rate. Its high cellulose content makes water hyacinth a potential source of cellulose nanofiber (CNF) for alternative commercial polymers that are difficult to degrade by nature. CNF isolation that only involves chemical treatment in purifying cellulose generally uses chemicals that are less environmentally friendly. In this study, steam explosion pretreatment was used to optimize the chemical treatment in cellulose purification and ultrasonication defibrillation in CNF isolation. The removal of FTIR spectra at peaks of 1730 cm-1, 1510 cm-1, and 1260 cm-1 as well as the drastic increase of crystallinity index in XRD and degradation temperature in TGA indicated that the chemical treatmen used successfully removed lignin and hemicellulose. At ultrasonication defibrillation time variations of 1, 2, and 3 hours, CNF with diameters of 24.30±0.62, 12.06±0.34, and 8.9±0.26 nm were produced where the diameter reduction was supported by an increase in the contact angle value. The percent yield of CNF at various ultrasonication times was 98%, 96%, 92%, respectively, and the slight decrease in the crystallinity index and degradation temperature of CNF of about 71% and 304ºC indicate that the ultrasonication method has little impact on crystal destruction and shortening of cellulose chains. Comparison with previous studies shows steam explosion pretreatment successfully reduces and simplifies the use of chemicals by damaging the initial structure of lignocellulose. The visual analysis and stability of the suspension dispersion, nanofiber diameter, FTIR spectra, crystallinity index, contact angle and thermal properties of the CNF produced in this study are comparable to previous studies so that the ultrasonication method is effective due to the lower mechanical defibrillation power used.
    URI
    https://repositori.usu.ac.id/handle/123456789/96743
    Collections
    • Undergraduate Theses [1308]

    Repositori Institusi Universitas Sumatera Utara (RI-USU)
    Universitas Sumatera Utara | Perpustakaan | Resource Guide | Katalog Perpustakaan
    DSpace software copyright © 2002-2016  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    Atmire NV
     

     

    Browse

    All of USU-IRCommunities & CollectionsBy Issue DateTitlesAuthorsAdvisorsKeywordsTypesBy Submit DateThis CollectionBy Issue DateTitlesAuthorsAdvisorsKeywordsTypesBy Submit Date

    My Account

    LoginRegister

    Repositori Institusi Universitas Sumatera Utara (RI-USU)
    Universitas Sumatera Utara | Perpustakaan | Resource Guide | Katalog Perpustakaan
    DSpace software copyright © 2002-2016  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    Atmire NV